PRODUCTS & TECHNOLOGY
Recommended
Surface adjustment
Details
Product Grade | Appearance | Product Usage | Features | Product process |
M-AC 1005 | White Powder | Pretreatment before coating: zinc based phosphating of ; surface container | Colloidal phosphopeptide system reduces phosphorylation reaction time, Product stability, Multi-metal adaptability |
Time: 0.5-1.0min. Temperature: 25-40℃ Pressure: 0.5-1.5bar Concentration: 0.1-0.2% |
M-AC 1006 | White Viscous Liquid | Pretreatment before coating: zinc based phosphating of ; surface container | Zinc phosphate system has strong liquid surface regulation activity and reduces the phosphating temperature to 40°C |
Time: 0.5-1.0min. Temperature: 25-40℃ Pressure: 0.5-1.5bar Concentration: 0.05-0.1% |
M-AC 1191 | Transparent Liquid | Surface container for aluminum and its alloy before passivation | Strong ability to adjust to aluminum and its aluminum alloy, Good light output effect, High cost performance |
Time: 2.0-10.0min. Temperature: 30-55℃ Pressure: 0.5-1.5bar Concentration: 1.0-3.0% |
M-AC 1202 | White Powder | Manganese series surface conditioner before phosphating | Manganese phosphate system refining phosphating crystal size and improving phosphating blackness |
Time: 0.5-1.0min. Temperature: 25-40°C Pressure: 0.5-1.5bar Concentration: 0.1-0.3% |
Inquire Now
*Note: Please make sure to fill in the information accurately and maintain smooth communication. We will contact you as soon as possible.
Customer service hotline:13696517500/13917913722
Service time:8:00-18:00
Sweep and follow us