PRODUCTS & TECHNOLOGY
Recommended
Aluminum wheel coating
Function positioning:
Surface treatment of passenger car aluminum wheels before powder coating
Application scenario:
Parts aluminum wheel manufacturing plant
Application substrate:
aluminum
Value advantage:
Significantly improve the bonding force and corrosion resistance of aluminum parts after powder spraying;
Damp heat test:
No obvious blisters after 96 hours at 37°C-100% relative humidity;
Salt spray experiment:
5% salt solution 35 ℃ 1000 hours test unilateral corrosion can not be greater than 3mm without obvious blisters;
CASS Karnofsky test:
5% salt solution plus copper chloride and acetic acid for 168 hours in the experiment, the unilateral corrosion should not be greater than 3mm without obvious blisters;
Fibrous corrosion test:
6-hour Karnofsky test (45 degree angle, 2-3 seconds water washing) 672-hour damp heat test (60°C 85% relative humidity) to measure the maximum fibrous corrosion length every week (scratch spacing of 40 mm can not be greater than 4 mm after standardization) Currently in the United States The laboratory calibration factor is 1.2)
Automobile and Parts - Aluminum Wheel Coating - Surface Treatment 1
Automobile and Parts - Aluminum Wheel Coating - Surface Treatment 2
Customer service hotline:13696517500/13917913722
Service time:8:00-18:00
Sweep and follow us
Copyright ©Shanghai Guanghua Shine Metal Surface Treatment CO., LTD